VESTAMID? D X9325
Polyamide 612
Characterization: 40% glass fiber reinforced, heat-stabilized
Applications: plastic-rubber composites
Its advantages over PA 12 exhibit in the
The PA 612 compounds of the VESTAMID? D series consequently represent specialty products that complement the comprehensive selection of PA 12 compounds of the VESTAMID? L series.
Filler / Reinforcement | |
Additive | |
Features | |
Agency Ratings | |
Appearance | |
Forms | |
Processing Method | |
Density (73°F) | 1.37 | g/cm3 | ISO 1183 |
Molding Shrinkage 2 |
|
| ISO 294-4 |
Across Flow | 0.80 | % |
|
Flow | 0.23 | % |
|
Water Absorption |
|
| ISO 62 |
Saturation, 73°F | 1.9 | % |
|
Equilibrium, 73°F, 50% RH | 0.80 | % |
|
Tensile Modulus | 1.36E+6 | psi | ISO 527-2/1A |
Tensile Stress (Break) | 21800 | psi | ISO 527-2/1A |
Tensile Strain (Break) | 4.0 | % | ISO 527-2/1A |
Charpy Notched Impact Strength |
|
| ISO 179/1eA |
-22°F, Complete Break | 7.6 | ft·lb/in2 |
|
73°F, Complete Break | 10 | ft·lb/in2 |
|
Charpy Unnotched Impact Strength |
|
| ISO 179/1eU |
-22°F, Complete Break | 49 | ft·lb/in2 |
|
73°F, Complete Break | 48 | ft·lb/in2 |
|
Heat Deflection Temperature |
|
|
|
66 psi, Unannealed | 410 | °F | ISO 75-2/B |
264 psi, Unannealed | 383 | °F | ISO 75-2/A |
Melting Temperature 3 | 414 | °F | ISO 11357-3 |
CLTE - Transverse (73 to 131°F) | 2.8E-5 | in/in/°F | ISO 11359-2 |
Flammability Classification |
|
| IEC 60695-11-10, -20 |
0.06 in | HB |
|
|
0.13 in | HB |
|
|
ISO Shortname | PA12, MH, 14-100, GF40 |
| ISO 1874 |