亚洲日韩久久综合中文字幕 ,精品国产免费一区二区三区香蕉,久久人人爽人人爽人人片DVD,精品人体无码一区二区三区

Products

Texin? 1210

Texin? 1210

Manufacturer: Covestro
Produced At:
 Europe / China
Product Category: TPU
Product No: Texin 1210 
Product Quantity: 25KG / BAG
Product Features: 
Abrasion Resistant,Chemical Resistant,F(xiàn)ood Contact Acceptable,Low Gel,Medium Clarity,Oil Resistant,Solvent Resistant

Texin? 1210

Thermoplastic Polyurethane Elastomer (Polyester)
Product Description:

Texin 1210 resin is an aromatic polyester-based thermoplastic polyurethane with a Shore hardness of approximately 92A.


Features 
  • Abrasion Resistant,Chemical Resistant,F(xiàn)ood Contact Acceptable,Low Gel,

  • Medium Clarity,Oil Resistant,Solvent Resistant

Uses 
  • Cable Jacketing,F(xiàn)ilm,F(xiàn)ootwear,Hose,Profiles,Sheet,Tubing
Agency Ratings 
  • FDA 21 CFR 177.1680,F(xiàn)DA 21 CFR 177.2600 
Appearance 
  • Natural Color

Processing Method 
  • Extrusion,Injection Molding 
Physical
Nominal Value
Unit
Test Method
Density / Specific Gravity



--
1.22

ASTM D792
--
1.22
g/cm3
ISO 1183
Hardness
Nominal Value
Unit
Test Method
Durometer Hardness (Shore A)
92

ASTM D2240, ISO 868
Mechanical
Nominal Value
Unit
Test Method
Flexural Modulus


ASTM D790, ISO 178
73°F
10600
psi

158°F
4600
psi

Taber Abrasion Resistance



1000 Cycles, 1000 g, H-18 Wheel
27.0
mg
ASTM D1044
1000 Cycles, 1000 g, H-18 Wheel
27.0
mg
ISO 4649
Elastomers
Nominal Value
Unit
Test Method
Tensile Stress


ASTM D412, ISO 37
100% Strain
1410
psi

300% Strain
2900
psi

Tensile Strength (Yield)
5800
psi
ASTM D412, ISO 37
Tensile Elongation (Break)
510
%
ASTM D412, ISO 37
Tear Strength



-- 2
737
lbf/in
ASTM D624
--
740
lbf/in
ISO 34-1
Compression Set 3


ASTM D395B, ISO 815
73°F, 22 hr
16
%

158°F, 22 hr
43
%

Thermal
Nominal Value
Unit
Test Method
Glass Transition Temperature
6.80
°F
DMA
Vicat Softening Temperature
190
°F
ISO 306/50, ASTM D1525 4
Injection
Nominal Value
Unit

Drying Temperature - Desiccant Dryer
178 to 219
°F

Drying Time - Desiccant Dryer
2.0
hr

Suggested Max Moisture
< 0.030
%

Suggested Max Regrind
20
%

Rear Temperature
360 to 385
°F

Middle Temperature
370 to 399
°F

Front Temperature
379 to 405
°F

Nozzle Temperature
385 to 410
°F

Processing (Melt) Temp
376 to 399
°F

Mold Temperature
61 to 100
°F

Injection Pressure
6000 to 15000
psi

Injection Rate
Moderate


Back Pressure
< 800
psi

Screw Speed
40 to 80
rpm

Cushion
< 0.125
in

Injection Notes
Hold Pressure: 60 to 80% of Injection Pressure
Extrusion
Nominal Value
Unit

Drying Temperature
178 to 219
°F

Drying Time
2.0
hr

Suggested Max Regrind
20
%

Cylinder Zone 1 Temp.
360 to 390
°F

Cylinder Zone 2 Temp.
360 to 399
°F

Cylinder Zone 3 Temp.
360 to 399
°F

Melt Temperature
376 to 399
°F

Die Temperature
370 to 399
°F



Products are widely used in plastic modification, automotive, construction, electrical and electronic, industrial, daily necessities and other fields