Stanyl? TC168 (NC239B)
聚酰胺 46
產(chǎn)品說明:
Thermal conductive material, Flame Retardant, Heat Stabilized, 20% Glass Reinforced
Special Features:
Used In:
Stanyl? is our high-performance polyamide 46 used for applications in automotive, E&E, gears and outdoor power equipments.
Stanyl is a high performance polyamide that provides unmatched performance and value for demanding applications in which superior heat resistance, design stiffness, wear & friction and process flow qualities are required.
Because Stanyl retains its mechanical properties at high temperatures up to 220°C, this makes it ideal for extremely high-performance applications, where it outperforms PPA, PA6T, PA9T, and often PPS and LCP.
填料/增強(qiáng)材料 | |
添加劑 | |
特性 | |
用途 | |
加工方法 | |
樹脂ID (ISO 1043) | |
密度 | 1.87 | g/cm3 | ISO 1183 |
收縮率 |
|
| ISO 294-4 |
橫向流量 | 0.60 | % |
|
流量 | 0.25 | % |
|
拉伸模量 | 2.03E+6 | psi | ISO 527-2 |
拉伸應(yīng)力 (斷裂) | 16700 | psi | ISO 527-2 |
拉伸應(yīng)變 (斷裂) | 1.6 | % | ISO 527-2 |
簡支梁缺口沖擊強(qiáng)度 |
|
| ISO 179/1eA |
-22°F | 3.6 | ft·lb/in2 |
|
73°F | 3.8 | ft·lb/in2 |
|
簡支梁無缺口沖擊強(qiáng)度 |
|
| ISO 179/1eU |
-22°F | 11 | ft·lb/in2 |
|
73°F | 11 | ft·lb/in2 |
|
熱變形溫度 (264 psi, 未退火) | 417 | °F | ISO 75-2/A |
熔融溫度 2 | 554 | °F | ISO 11357-3 |
線形熱膨脹系數(shù) |
|
| ISO 11359-2 |
流動(dòng) | 1.2E-5 | in/in/°F |
|
橫向 | 1.4E-5 | in/in/°F |
|
導(dǎo)熱系數(shù) |
|
| ASTM E1461 |
-- 3 | 6.2 | Btu·in/hr/ft2/°F |
|
-- 4 | 15 | Btu·in/hr/ft2/°F |
|
漏電起痕指數(shù) | 300 | V | IEC 60112 |
可燃性等級 (0.03 in) | V-0 |
| IEC 60695-11-10, -20 |
干燥溫度 | 176 | °F |
干燥時(shí)間 | 2.0 | hr |
料筒后部溫度 | 536 到 608 | °F |
料筒中部溫度 | 572 到 608 | °F |
料筒前部溫度 | 572 到 608 | °F |
射嘴溫度 | 581 到 635 | °F |
加工(熔體)溫度 | 581 到 617 | °F |
模具溫度 | 176 到 248 | °F |
注射速度 | 中等偏快 |
|
背壓 | 290 到 1450 | psi |
螺桿壓縮比 | 2.5:1.0 |
|