Desmopan? 445
熱塑性聚氨酯彈性體(聚酯)
injection molding grade; grease and oil-resistant; good heat resistance; low compression set; Application; Automotive engineering; Injection molded engineering parts
密度 |
|
|
|
73°F | 1.22 | g/cm3 | ISO 1183 |
-- | 0.0441 | lb/in3 | ISO 1183 2 |
肖氏硬度 |
|
|
|
邵氏 A, 1 秒, 73°F | 93 |
| ISO 7619 |
邵氏 D, 1 秒, 73°F | 44 |
| ISO 7619 |
邵氏 A, 3 sec | 93 |
| ISO 868 2 |
邵氏 D, 15 sec | 44 |
| ISO 868 2 |
拉伸應(yīng)力 3 |
|
| DIN 53504 |
斷裂, 73°F | 8180 | psi |
|
10% 應(yīng)變, 73°F | 798 | psi |
|
50% 應(yīng)變, 73°F | 1680 | psi |
|
100% 應(yīng)變, 73°F | 2070 | psi |
|
300% 應(yīng)變, 73°F | 4570 | psi |
|
拉伸應(yīng)變 3 (斷裂, 73°F) | 490 | % | DIN 53504 |
Tensile Storage Modulus |
|
| ISO 6721 |
-4°F | 115 | ksi |
|
68°F | 14.9 | ksi |
|
140°F | 8.41 | ksi |
|
Torsional Storage Modulus |
|
| ISO 6721 |
-4°F | 40611 | psi |
|
73°F | 3626 | psi |
|
158°F | 2321 | psi |
|
抗磨損性 4 | 25.0 | mm3 | ISO 4649 |
撕裂強(qiáng)度 5 (73°F) | 540 | lbf/in | ISO 34-1 |
壓縮永久變形 |
|
| ISO 815 |
73°F, 72 hr | 25 | % |
|
158°F, 24 hr 4 | 35 | % |
|
Rebound Resilience | 35 | % | ISO 4662 |
干燥溫度 | < 230 | °F |
|
加工(熔體)溫度 | 410 到 455 | °F |
|
模具溫度 | 68 到 104 | °F |
|